The price gap between ground and unground rod is 30 to 50 percent. Sometimes that is money well spent, sometimes it is a habit. Here is how to tell which case you are in.

Every week someone asks us to quote both options, then picks the cheaper one without quite knowing what they gave up. Ground and unground rod are the same material out of the same furnace. The difference is what happens afterwards, and whether that matters depends on the next operation.

What unground rod actually is

Rod comes out of the sintering furnace at a diameter slightly larger than nominal, with a surface skin that has seen the graphite environment rather than the grinding wheel. Diameter typically runs +0.3 to +0.5 mm. There is a slight bow, usually within 0.1–0.3 mm over 330 mm, and the surface hardness in the outer 0.1 mm can be a point or two lower because some cobalt has evaporated at the surface.

None of this is a defect. It is the natural state of a sintered part, and it is perfectly usable if the next step removes the skin anyway.

What grinding adds

Centerless grinding takes the rod down to nominal, removes the decarburised layer, and corrects the bow. A properly ground h6 rod gives you:

  • Diameter tolerance inside 0.013 mm for a 10 mm rod (h6), and 0.011 mm for h5.
  • Roundness typically within 0.002 mm.
  • Straightness around 0.02 mm per 100 mm, sometimes 0.01 mm on premium stock.
  • Surface finish Ra 0.2–0.4 µm, which is enough to grip in a collet without marking.

That last point matters more than buyers expect. An unground rod in a 5C collet contacts the surface at a few high spots. Under cutting load it can shift, and the runout you measured at setup is not the runout you get at 12,000 rpm.

When unground is the right call

Unground rod is fine, and often preferable, in these cases:

  1. The rod will be cut and brazed. Brazing destroys the surface anyway, and the joint gap is controlled by the fixture, not the rod tolerance.
  2. The rod goes into EDM. Wire EDM does not care about the outer 0.3 mm, and the setup is dialled in from the machine, not the stock.
  3. The part is a wear block that gets surface ground after assembly. You are paying twice if you buy ground stock and then grind it again.
  4. The diameter is large. Above 25 mm, the price premium per kilogram grows faster than the benefit, and many shops simply turn or grind the blank themselves.

When the premium pays for itself

Buy ground when the rod goes straight into a precision operation with no intermediate sizing step:

  • Tool blanks for CNC flute grinding, where blank runout transfers directly into radial runout.
  • Guide pins, needles and small shafts that must slide in a bore.
  • Plungers and seal surfaces, where finish and roundness control leakage.
  • Any automatic bar feeder, because a bowed rod jams a magazine faster than a dull tool.

There is also a hidden saving. Ground rod lets you skip a rough grinding pass, which is often 20–40 minutes of machine time per piece on a manual grinder. If your hourly rate is meaningful, the material premium can pay back inside one batch.

The thin-wall exception

Ground tube and thin-wall rod behave differently. When the wall drops below 1 mm, centerless grinding can distort the section, and you may see ovality instead of roundness. For thin-wall tube with a small bore, it is often better to buy near-net sintered stock and finish it on a mandrel. Tell the supplier the wall thickness at quoting stage; it changes the process, not just the tolerance.

How to check what you received

Three measurements catch most problems:

Diameter at three points along the length, rotated 90° between readings. A two-point check will miss ovality.

Straightness on a surface plate, rolling the rod under a dial indicator. Do it on the full length, not a 100 mm sample, if the rod will be fed automatically.

Surface under a low-power loupe. Pits, darker patches or a visible seam along the length suggest the skin was not fully removed or the density is low. A ground rod should look uniform along its whole length.

Price, put plainly

For a 10 mm rod in 10% cobalt, unground might sit around a base price per kilogram. Ground h6 typically adds 30–50% depending on diameter and straightness class, because centerless grinding is a slow, wheel-consuming operation and the yield loss is real. Below 3 mm, the premium is steeper, since small diameters are harder to hold and inspect.

We quote both forms from the same sinter-HIP stock, so the grade and density do not change when you choose unground to save money. You can see the tolerance options on the ground tungsten carbide rod pages, including h6 and h5 stock with 0.02 mm straightness, and the unground equivalents alongside them.

Grade choice still has to come first. The grade and grain size guide explains why a sub-micron rod may grind worse on a machine set up for medium grain, which is a common reason a tolerance upgrade fails to deliver.

If you are not sure which way to go, describe the next three operations after the rod arrives. That is usually enough to decide, and it is a shorter conversation than a returned pallet. A typical starting point is this YL10.2 ground rod with a 0.15 mm hole, which shows the tolerance and finish we hold on small bores.